Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 560 MPa | >= 81200 psi | Minimum Guaranteed |
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Tensile Strength, Yield | 560 MPa @Strain 0.200 % |
81200 psi @Strain 0.200 % |
|
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Tensile Strength, Yield | 560 MPa @Strain 0.200 % |
81200 psi @Strain 0.200 % |
|
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 560 MPa @Strain 0.200 % |
81200 psi @Strain 0.200 % |
Typical |
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |
|||
Tensile Strength, Yield | 560 MPa @Strain 0.200 % |
81200 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |