Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM D638 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM value at 50 mm/min. |
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose nylon 6 exhibiting excellent fluidity for filling thin sections. It possesses the combination.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM value at 50 mm/min. |
BASF Capron® 8203C Nylon 6 (Dry)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | d.a.m.; ISO 527-1, -2; 50 mm/min |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features include Easy Molding, Mold Release. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM-D638 |
Polyram PlusTek PA604 Nylon 6.6, Heat Stabilized High heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527 |
Polyram PlusTek PA700BL10 Nylon 6.6 for Injection Molding, UV Stabilized UV Stabilized Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527 |
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR Information provided by EMS Grivory |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50 mm/min; ISO 527 |
Eurostar Staramide A28 PA66, Injection Molding Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM D638 |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics .. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO R 527 |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50 [mm/min], Test Speed 50 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50mm/min; ISO 527-2 |
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50 mm/min |
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant
(discontinued **) OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50 mm/min |
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |
|||
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |