Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ1022 PC Standard Flow OQ Resin |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific) Standard Flow OQ Resin |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® OQ3820 PC High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 61.0 MPa @Temperature 23.0 °C |
8850 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**) Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM941A PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | ASTM D638 |
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50mm/min; ISO 527 |
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ASAPC GLY 130 UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | ASTM D638 |
Ashley Polymers Ashlene® R528LW Nylon 66 General purpose injection molding grade Nylon 66, lubricated and FDA approved.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |
|||
Tensile Strength, Yield | 61.0 MPa | 8850 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |