Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 29.0 - 90.3 MPa | 4210 - 13100 psi | Average value: 64.1 MPa Grade Count:18 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Tensile Strength, Yield | 43.4 - 90.3 MPa | 6300 - 13100 psi | Average value: 75.3 MPa Grade Count:22 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |