Polymer Property : Tensile Strength, Yield = 9000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 - 62.1 MPa
8000 - 9000 psi
ASTM D638
Alcoa KAMA 4100 Prime APET  (discontinued **)
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,..
Tensile Strength, Yield 34.5 - 62.1 MPa
5000 - 9000 psi
ASTM D638
Alcoa KAMA 5100 CPET  (discontinued **)
CapabilitiesGauge: .020" to .040" (508 to 106µm)Width: 20" to 52" (508 to 1321mm)Core size: 3" or 6"Roll O.D.: 29" standard, available up to 40"Silicone coating availableAvailable in natural blackP..
Tensile Strength, Yield 1.38 - 62.1 MPa
200 - 9000 psi
Average value: 23.2 MPa Grade Count:13
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..