Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced Excellent Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
PTS Trimid® N66-1010 Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D882 |
Honeywell Capran® 526 Heat-Stabilized Nylon Film, Blown Tubular Film
(discontinued **) Description: Capran® 526 is a blue-tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 60 inches as layflat tubing and 120 inches as slit tubing... |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | .01% permanent set |
Meehanite GF-20 Flake Graphite Cast Iron Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR-N HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6,6 GF NAT Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PA11 Availability: North AmericaForms: PelletsFeatures: Medium ViscosityTPCI# 6486106Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PA12 L N MB Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 TS18 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES Luriblend® TPX-POM-01060 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM Data |
Styron CALIBRE™ 603 3 Polycarbonate, Branched CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high m.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ISO R527 type 1 |
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix HexPly® 913 is a proven modified epoxy matrix with a low temperature cure cycle which exhibits outstanding environmental resistance, whilst retaining good hot/wet mechanical performance. This versa.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | >= 65.5 MPa | >= 9500 psi | ASTM D638 |
Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-25FG-1734 25% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |