Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Meehanite GF-20 Flake Graphite Cast Iron

Category Metal , Ferrous Metal , Cast Iron , Gray Cast Iron
Manufacturer Meehanite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meehanite GF-20 Flake Graphite Cast Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Physical Properties Metric English Comments
Specific Gravity 6.80 g/cc
6.80 g/cc
Mechanical Properties Metric English Comments
Hardness, Brinell 150
150
Nominal
Tensile Strength, Ultimate 138 MPa
20000 psi
Tensile Strength, Yield 65.5 MPa
9500 psi
.01% permanent set
Modulus of Elasticity 62.1 GPa
9000 ksi
Compressive Strength 621 MPa
90000 psi
Poissons Ratio 0.24
0.24
Fatigue Strength 75.8 MPa
11000 psi
Machinability 30 %
30 %
Dalcher
Shear Modulus 27.6 GPa
4000 ksi
Shear Strength 148.6 MPa
21550 psi
Izod Impact Unnotched 5.42 - 12.2 J

@Diameter 20.3 mm
4.00 - 9.00 ft-lb

@Diameter 0.798 in
Thermal Properties Metric English Comments
Shrinkage 0.80 %
0.80 %
Patternmaker Shrinkage
Users viewing this material also viewed the following: