Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPC-40G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced Excellent Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 65.5 - 119 MPa | 9500 - 17300 psi | Average value: 90.8 MPa Grade Count:9 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Global GAB-110 10% Glass Reinforced, General Purpose ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | .01% permanent set |
Meehanite GF-20 Flake Graphite Cast Iron Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6,6 GF NAT Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Spartech Polycast SAR HP 1.25 (UL 752 Level 3) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 TS18 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES Luriblend® TPX-POM-01060 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4731-8 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PA12 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Chase Plastics CP Pryme® PC110R Polycarbonate, 10% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ISO R527 type 1 |
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix HexPly® 913 is a proven modified epoxy matrix with a low temperature cure cycle which exhibits outstanding environmental resistance, whilst retaining good hot/wet mechanical performance. This versa.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | >= 65.5 MPa | >= 9500 psi | ASTM D638 |
Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ES-000/15T Polyethersulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |