Mechanical Properties Metric English Comments
Tensile Modulus 0.260 GPa

@Temperature 23.0 °C
37.7 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET  (Unverified Data**)
Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t..
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2420 F LDPE
Film, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2420 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2420 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2425 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2426 F LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2441 D LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.260 GPa
37.7 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer
LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant.
Tensile Modulus 0.260 GPa
37.7 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific)
LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications.
Tensile Modulus 0.260 GPa
37.7 ksi
TD; ASTM D882-A
Borealis FT5230 Low Density Polyethylene
FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: ..
Tensile Modulus 0.260 GPa
37.7 ksi
TD; ASTM D882-A
Borealis FT5231 Low Density Polyethylene
FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d..
Tensile Modulus 0.260 GPa
37.7 ksi
TD; ASTM D882-A
Borealis FT5232 Low Density Polyethylene
FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op..
Tensile Modulus 0.260 GPa
37.7 ksi
TD; ASTM D882-A
Borealis FT5236 Low Density Polyethylene
FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic..
Tensile Modulus 0.260 GPa
37.7 ksi
ISO 527-1/-2
DSM Arnitel® EM631-HB TPC-ET
Extrusion Grade, Heat Stabilized
Tensile Modulus 0.260 GPa
37.7 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® SC969 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Tensile Modulus 0.260 GPa
37.7 ksi
MD
BASF Ultramid® B32 0.015 BOPA Film
Information provided by BASF
Tensile Modulus 0.260 GPa
37.7 ksi
MD
Kuraray HYBRAR® BF1 Three Layer Blown Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w..
Tensile Modulus 0.260 GPa
37.7 ksi
LyondellBasell Lupolen® 2424 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.