Material Notes:
FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications FT5231 has been developed especially for applications like: shrink film, carrier-bag film, lamination films, and food packaging.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ISO 527-3
Film Elongation at Break, TD 550 %
550 %
ISO 527-3
Tensile Modulus 0.230 GPa
33.4 ksi
MD; ASTM D882-A
0.260 GPa
37.7 ksi
TD; ASTM D882-A
Puncture Energy 2.50 J
1.84 ft-lb
66N; ASTM D5748
Coefficient of Friction 0.80
0.80
Dynamic; ISO 8295
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Elmendorf Tear Strength, TD 5.097 g/micron
129.5 g/mil
ISO 6383/2
Dart Drop Test 120 g

@Thickness 0.0400 mm
0.265 lb

@Thickness 0.00157 in
ISO 7765-1
Film Tensile Strength at Break, MD 27.0 MPa
3920 psi
ISO 527-3
Film Tensile Strength at Break, TD 24.0 MPa
3480 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 112 °C
234 °F
ISO 11357-3
Vicat Softening Point 97.0 °C
207 °F
ISO 306
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM D1003
Gloss 85 %
85 %
ASTM D2457