Tensile Modulus 1.17 GPa
170 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Flint Hills P6G2Z-090 Impact Copolymer Polypropylene
Features: Excellent impact strength and weldability. Product does not contain animal derived components.Applications: Injection Molding and thermoforming - Automotive coolant bottlesInformation p..
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE
Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri..
Tensile Modulus 1.17 GPa
170 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific)
A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications
Tensile Modulus 1.17 GPa
170 ksi
2 in/min; ASTM Test
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
Tensile Modulus 1.17 GPa
170 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Tensile Modulus 1.17 GPa
170 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Tensile Modulus 1.17 GPa
170 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP
PPE+PP blend. Suitable for painted exterior automotive applications.
Tensile Modulus 1.17 GPa
170 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific)
PPE+PP blend. Suitable for painted exterior automotive applications.
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Westlake Plastics Propylux® Void-Free Polypropylene
Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance to abrasion. These properties make it suitable fo..
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding
Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an a..
Tensile Modulus 1.17 GPa
170 ksi
2 in/min; ASTM D638
ExxonMobil HDPE HYA 800 High Density Polyethylene Resin
Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal ..
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Ensinger Tecapeek® XP-104 Compression Molded PEEK Compound, with 7% Molybdenum Disulfide, 3% PTFE and 25% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Modulus 1.17 GPa
170 ksi
1 mm/min
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent...
Tensile Modulus 1.17 GPa
170 ksi
1 mm/min
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry)
Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to ..
Tensile Modulus 1.17 GPa
170 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 527
Arkema Group Rilsamid® PA 12 AMNO MED Nylon 12
Rilsamid® AMNO MED is a thermoplastic polyamide 12. This grade dedicated to injection offers the highest quality and it is specifically designed to meet the stringent requirements of the medical ap..
Tensile Modulus 1.17 GPa
170 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MS000IL PP
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c..