ExxonMobil HDPE HYA 800 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HYA 800 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: Yes Applications: Drainage PipesFood packagingLiquid Food Containers for Milk, Water and Juices Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ASTM D4883
ESCR 100% Igepal® 20 hour
20 hour
F50; ASTM D1963
ESCR 10% Igepal® <= 20 hour
<= 20 hour
F50; ASTM D1963
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
46 g/10 min

@Load 21.6 kg,
Temperature 190 °C
46 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64

@Time 15.0 sec
64

@Time 0.00417 hour
ASTM D2240
Tensile Stress 13.8 MPa

@Strain 100 %
2000 psi

@Strain 100 %
2 in/min; ASTM D412
Tensile Strength, Yield 29.0 MPa
4200 psi
2 in/min; ASTM D638
Elongation at Break >= 100 %
>= 100 %
2 in/min; ASTM D638
Tensile Modulus 1.17 GPa
170 ksi
2 in/min; ASTM D638
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.70 ft-lb/in²
Area; ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 129 °C
264 °F
ASTM D1525