Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1050 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 7.24 GPa
1050 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Modulus 7.21 GPa
1050 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Konduit MT00EL PP
LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th..
Tensile Modulus 7.24 GPa
1050 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
Tensile Modulus 7.22 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC (Asia Pacific)
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.
Tensile Modulus 7.22 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC
LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Tensile Modulus 7.22 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Tensile Modulus 7.25 GPa
1050 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® DP 2037/30 H2.0 LT 904040 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, black colored for laser transmission-welding (laser-transparent), good heat-ageing resistance
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer
LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
Tensile Modulus 7.21 GPa
1050 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP ZFL34 PPE+PS
LNP* LUBRICOMP* ZFL34 is a compound based on PPE+PS resin containing 20% Glass Fiber, 15% PTFE. Added feature of this gradae is: Wear Resistant.
Tensile Modulus 7.21 GPa
1050 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO
LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Asia Pacific)
LNP* Stat-kon* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 7.27 GPa
1050 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX11411 PC
LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Tensile Modulus 7.24 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET
LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant.
Tensile Modulus 7.24 GPa
1050 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT
LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized.
Tensile Modulus 7.25 GPa
1050 ksi
Film T.D.; ASTM D882
Eastman Eastman Embrace Copolyester for Shrink Film
Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood ..
Tensile Modulus 7.26 GPa
1050 ksi
Storage
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E2101 is a two component, thixotropic, electrically conductive adhesive. It may be used for circuit assembly and semiconductor applications. Advantages & Application ..
Tensile Modulus 7.25 GPa
1050 ksi
ISO 527
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..