Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.72 - 7.93 GPa | 1120 - 1150 ksi | 20% Glass Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Tensile Modulus | 7.72 - 7.93 GPa | 1120 - 1150 ksi | 20% Glass Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |