Mechanical Properties Metric English Comments
Tensile Modulus 128 GPa
18500 ksi
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Tensile Modulus 128 GPa
18500 ksi
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Tensile Modulus 128 GPa
18500 ksi
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Tensile Modulus 128 GPa
18500 ksi
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..