Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 128 GPa | 18500 ksi | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Modulus | 128 GPa | 18500 ksi | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Modulus | 128 GPa | 18500 ksi | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Modulus | 128 GPa | 18500 ksi | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |