Polymer Property : Tensile Modulus = 15.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.103 GPa
15.0 ksi
ISO 527-2/1A/1
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade)
Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East..
Tensile Modulus 0.103 GPa
15.0 ksi
ISO 527-2/1A/1
ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade)
Product Description: LD 655 is a very high flow LDPE grade with a very good flexibility. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabiliz..
Tensile Modulus 0.103 GPa
15.0 ksi
Molded Properties; ISO 527-2/1A/1
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b..