ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Artificial FlowersCarpet BackingCompoundingInjection MoldingMasterbatch Base ResinInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.913 g/cc
0.0330 lb/in³
ExxonMobil method
Melt Flow 70 g/10 min
70 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
ISO 868
Tensile Strength at Break 6.89 MPa
1000 psi
ISO 527-2/1A/50
Elongation at Break 150 %
150 %
ISO 527-2/1A/50
Tensile Modulus 0.103 GPa
15.0 ksi
ISO 527-2/1A/1
Thermal Properties Metric English Comments
Melting Point <= 214 °C
<= 417 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 75.0 °C
167 °F
ISO 306