Mechanical Properties Metric English Comments
Tensile Modulus 15.1 GPa
2190 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber
Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient..
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Tensile Modulus 15.1 GPa
2190 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Tensile Modulus 15.1 GPa
2190 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
Tensile Modulus 15.1 GPa
2190 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON EV008 PEI
LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural.
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber
Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn..
Tensile Modulus 15.1 GPa
2190 ksi
ASTM-D790
Polyram Polytron P60B01 Homopolymer Polypropylene, Chemically Coupled 60% LGF
A chemically coupled 60% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Tensile Modulus 15.1 GPa
2190 ksi
ASTM-D790
Polyram Polytron P60B11 Homopolymer Polypropylene, Chemically Coupled 60% LGF
A chemically coupled 60% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.
Tensile Modulus 15.1 GPa
2190 ksi
ASTM D638
Plenco 5350 Phenolic, Granular, Compression Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of ..
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers.