Polymer Property : Tensile Modulus = 16.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 16.8 GPa
2440 ksi
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Tensile Modulus 16.8 GPa

@Temperature 23.0 °C
2440 ksi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Tensile Modulus 16.8 GPa
2440 ksi
ASTM D638
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Tensile Modulus 16.8 GPa

@Temperature 23.0 °C
2440 ksi

@Temperature 73.4 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Tensile Modulus 16.8 GPa
2440 ksi
ASTM D638
Plenco 6990 Phenolic, Briquette, Compression Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Tensile Modulus 16.8 GPa
2440 ksi
ASTM D638
Plenco 7556 Phenolic, Briquette, Injection Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..
Tensile Modulus 16.8 GPa
2440 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50
Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory..
Tensile Modulus 16.8 GPa
2440 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
Tensile Modulus 16.8 GPa
2440 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Tensile Modulus 16.8 GPa
2440 ksi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
Fibre Glast RAE 2426 / 2177 Epoxy  (discontinued **)
Information provided by Fibre Glast Developments Corporation.
Tensile Modulus 16.8 GPa
2430 ksi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
Fibre Glast ProSet 125R / 229H Epoxy  (discontinued **)
Information provided by Fibre Glast Developments Corporation.