Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 180 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.24 GPa
180 ksi
100 micron film; ASTM D882
Kaneka PHBH Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU
LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity.
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP
High modulus/impact/heat PPE+PP
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific)
High modulus/impact/heat PPE+PP.
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7115F PPE+PP
High modulus/impact/heat PPE+PP. Compliant with US FDA food contact regulations for temperatures of use of room temperature and below.
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Tensile Modulus 1.24 GPa
180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Stat-Rite® M-690 is a static dissipative PETG alloy. Stat-Rite® M-690 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio..
Tensile Modulus >= 1.24 GPa
>= 180 ksi
Master Bond UV24TKLO One Component, UV-Curable, Low Outgassing Adhesive System
Master Bond Polymer System UV24TKLO is a one part UV curable epoxy modified formulation for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-5..
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer
TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th..
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade
Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for..
Tensile Modulus 1.24 GPa
180 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior ..
Tensile Modulus 1.24 GPa
180 ksi
1 mm/min
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Dry)
Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High ..
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Americas Styrenics EC6600 High Impact Polystyrene
Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy..
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat
Approved to GMP.PP.013
Tensile Modulus 1.24 GPa
180 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved