Material Notes:
Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength at Break 20.7 MPa
3000 psi
ASTM D638
Tensile Strength 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Flexural Strength 30.3 MPa
4400 psi
ASTM D790
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 0.876 J/cm
1.64 ft-lb/in
compression molded; ASTM D256
1.23 J/cm
2.30 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.3 °C
191 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.2 °C
171 °F
ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525