Mechanical Properties Metric English Comments
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437T20L1 Talc Reinforced
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336C10L1 Calcium Reinforced
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accucomp Polypropylene HPO306L Homopolymer
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0436T10L Talc Reinforced