Aclo Accucomp Polypropylene HPO306L Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polypropylene HPO306L Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength at Break 22.0 MPa
3190 psi
ASTM D638
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Flexural Strength 42.0 MPa
6090 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C
127 °F