Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60
60
ASTM D785
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.300 GPa
188.5 ksi
ASTM D638
Flexural Strength 24.0 MPa
3480 psi
ASTM D790
Flexural Modulus 1.100 GPa
159.5 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 52.2 °C
126 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F