Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit TX10916 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30 Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiff.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Barlog Plastics KEBATRON C1065X1 PPS, cross-linked, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |
|||
Tensile Modulus | 19.0 GPa | 2750 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |