Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific) LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 19.0 - 21.0 GPa | 2760 - 3050 ksi | ISO 527 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit TX10916 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H SST black 9288 PA12-GF65 Product description: Grilamid LV-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the f.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30 Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiff.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Barlog Plastics KEBATRON C1065X1 PPS, cross-linked, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |