Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.57 GPa | 373 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.57 GPa | 373 ksi | ISO 527 |
FKuR Kunststoff Terralene® WF 6534 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Tensile Modulus | 2.57 GPa | 373 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific) LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.57 GPa | 373 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.57 GPa | 373 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS (Asia Pacific) LNP* Thermocomp* AB002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Bead. |
|||
Tensile Modulus | 2.57 GPa | 373 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354P PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating performance, a good candidate for Laser Direct Structuring applications. |