SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* AB002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Bead.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Tensile Modulus 2.57 GPa
373 ksi
50 mm/min; ASTM D638
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.55 J/cm
12.3 ft-lb/in
ASTM D4812