Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.59 GPa | 376 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | ASTM D638 |
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 2.59 GPa @Temperature 23.0 °C |
376 ksi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC900 CPVC is an extrusion compound for CTS Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC900 demonstrates eas.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated
(discontinued **) Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP (Asia Pacific) LNP* Thermocomp* MB006HS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare. |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | ASTM D-882 |
Saint-Gobain Norton® High Performance Extruded PEI Film Description: PEI = polyetherimide. Used Primarily for Electrical/Electronics ApplicationsInformation provided by Saint Gobain Performance Products. |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | Storage |
Epoxy Technology EPO-TEK® E3001 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
Tensile Modulus | 2.59 GPa @Temperature 130 °C |
375 ksi @Temperature 266 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | ASTM D-638 |
Axiall ProTherm® 4303 Rigid PVC, Extrusion Georgia Gulf 4303 is a CPVC powder formulation designed for the processing of pipe products with an O.D. range of 1/2" to 8 inches requiring high heat deflection temperatures. Processing and stabil.. |
|||
Tensile Modulus | 2.59 - 3.28 GPa | 375 - 475 ksi | ASTM D638 |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Tensile Modulus | 2.59 - 3.28 GPa | 375 - 475 ksi | ASTM D638 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | ASTM Test |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Tensile Modulus | 2.59 GPa | 375 ksi | TM R050-36 |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Tensile Modulus | 2.59 GPa @Temperature 120 °C |
376 ksi @Temperature 248 °F |
ISO Data |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |