Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.190 GPa @Temperature 23.0 °C |
27.6 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | ASTM D882 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | ASTM D882 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | ASTM D882 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | ASTM D882 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | ASTM D882 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | ASTM D882 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | |
LyondellBasell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | MD/TD; ASTM D882-A |
Borealis FA3220 Low Density Polyethylene FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has bee.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | MD/TD; ASTM D882-A |
Borealis FA3227 Low Density Polyethylene FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | Bending Modulus; ASTM D790 |
UBE UMERIT 1500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Tensile Modulus | 0.190 GPa | 27.6 ksi | Bending Modulus; ASTM D790 |
UBE UMERIT 1520F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Tensile Modulus | >= 0.190 GPa | >= 27.6 ksi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |