Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 29.0 GPa | 4210 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-40LCF/001 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 29.0 GPa @Temperature 23.9 °C |
4200 ksi @Temperature 75.0 °F |
0° Direction, Dry; 18oz. Woven roving form; ASTM D638 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, Glass Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Tensile Modulus | 29.0 GPa | 4210 ksi | ISO 527-1 |
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa.. |
|||
Tensile Modulus | 29.0 GPa | 4210 ksi | ISO 527-1 |
Vyncolit X659 Glass, Mineral and Graphite Filled Novolac Phenolic Novolac resin based, glass fiber, mineral and graphite filled. Grade with superior stiffness, high dimensional stability and excellent tribological properties. Good chemical resistance against sever.. |
|||
Tensile Modulus | 29.0 GPa @Temperature 24.0 °C |
4210 ksi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric Hexcel designation: K285-38"-F522; Kev. 49 1140Information provided by HexCel |
|||
Tensile Modulus | 29.0 GPa | 4210 ksi | RT; Dry; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |