Polymer Property : Tensile Modulus = 3.95 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.95 GPa
573 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® INP562 ABS
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Modulus 3.95 GPa
573 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Modulus 3.95 GPa
573 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL4019 PC
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Tensile Modulus 3.95 GPa
573 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Tensile Modulus 3.95 GPa
573 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Tensile Modulus 3.95 GPa
573 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Tensile Modulus 3.95 GPa
573 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific)
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Tensile Modulus 3.95 GPa
573 ksi
1 mm/min; ISO 527-1,-2
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
Tensile Modulus 3.95 GPa
573 ksi
1 mm/min; ISO 527-1,-2
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..