Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3190 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 22.0 GPa
3190 ksi
ASTM D638
Gharda Chemicals GATONE™ 5630CF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Tensile Modulus 22.0 GPa
3190 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of..
Tensile Modulus 22.0 GPa

@Temperature 23.0 °C
3190 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Tensile Modulus 22.0 GPa
3190 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi..
Tensile Modulus 22.0 GPa
3190 ksi
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
Tensile Modulus 22.0 GPa
3190 ksi
ISO 527 Type 1A
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Modulus 22.0 GPa
3190 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
Tensile Modulus 22.0 GPa
3190 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s..
Tensile Modulus 22.0 GPa
3190 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive.
Tensile Modulus 22.0 GPa
3190 ksi
ISO 527-1
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60
Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60
Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60
Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60
Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following ..
Tensile Modulus 22.0 GPa
3190 ksi
1 mm/min; ISO 527
Eurostar Staramide ACF6 PA66, 30% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF6 is a 30% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 22.0 GPa
3190 ksi
ISO 527
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-6H black PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Tensile Modulus 22.0 GPa
3190 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60
Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Tensile Modulus 22.0 GPa
3190 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60
Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
Tensile Modulus 22.0 GPa
3190 ksi
ASTM D638
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60
Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
Tensile Modulus 22.0 GPa
3190 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-6H PA*-GF60
Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...