Polymer Property : Tensile Modulus = 336 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.32 GPa
336 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.32 GPa
336 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne
Tensile Modulus 2.32 GPa
336 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2798 Polyvinyl Chloride, Rigid (PVC, Rigid)
Premium chemical resistant Compound for Packaging.Information provided by PolyOne
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® 123X PC Copolymer
Improved flow PC with excellent processability and mold release.
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East)
Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East)
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Tensile Modulus 2.32 GPa
336 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Tensile Modulus 2.32 GPa
336 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Tensile Modulus 2.32 GPa
336 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.
Tensile Modulus 2.32 GPa
336 ksi
ASTM D638
Spartech Solarex® SV Copolyester Sheet
Description: Copolyester SheetInformation provided by Spartech.
Tensile Modulus 2.32 GPa
336 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific)
LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I..
Tensile Modulus 2.32 GPa
336 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon DS0029 PC
LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t..
Tensile Modulus 2.32 GPa
336 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.
Tensile Modulus 2.32 GPa

@Temperature 120 °C
336 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned)
Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G ..