Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Solarex® SV Copolyester Sheet

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Spartech
Trade Name Solarex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Solarex® SV Copolyester Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyester SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 48.80 MPa
7078 psi
ASTM D638
Tensile Modulus 2.32 GPa
336 ksi
ASTM D638
Flexural Yield Strength 85.998 MPa
12473 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Unnotched 0.523 J/cm
0.980 ft-lb/in
ASTM D256
0.294 J/cm

@Temperature -40.0 °C
0.550 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 75.6 µm/m-°C

@Temperature 20.0 °C
42.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.2 °C
153 °F
ASTM D648