Mechanical Properties Metric English Comments
Tensile Modulus 1.80 - 2.60 GPa

@Thickness 2.00 mm
261 - 377 ksi

@Thickness 0.0787 in
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF)
Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope..
Tensile Modulus 2.10 - 2.60 GPa
305 - 377 ksi
Goodfellow Polyvinyl Fluoride (PVF) Film
A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v..
Tensile Modulus 2.30 - 2.60 GPa
334 - 377 ksi
ASTM D638
3D Systems Accura® Xtreme White 200 Plastic
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl..