Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 379 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.61 GPa
379 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.61 GPa
379 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.61 GPa
379 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer
High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin
Tensile Modulus 2.61 GPa
379 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific)
High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
Tensile Modulus 2.61 GPa
379 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East)
High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
Tensile Modulus 2.61 GPa
379 ksi
1mm/min
Eastman Eastapak 9921W PET  (discontinued **)
Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Tensile Modulus 2.61 GPa
379 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East)
Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par..
Tensile Modulus 2.61 GPa
379 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
Tensile Modulus 2.61 GPa
379 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Tensile Modulus 2.61 GPa
379 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL NH5120 PPE+PS
Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re..
Tensile Modulus 2.61 GPa
379 ksi
Abatron AboCast 8103-25 High-Performance Dielectric Epoxy
AboCast 8103-25 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines o..
Tensile Modulus 2.61 GPa
379 ksi
ASTM D-638
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..
Tensile Modulus 2.61 GPa
379 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East)
High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.