Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
15 sec; ASTM D2240
Tensile Strength, Yield 43.9 MPa
6370 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.61 GPa
379 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 80.7 MPa
11700 psi
ASTM D790
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
Izod Impact, Notched 6.00 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
11.2 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
7.80 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
14.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
9.40 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
17.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy 55.6 J/cm

@Temperature 23.0 °C
0.104 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
199 J/cm

@Temperature 23.0 °C
0.373 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 3.18 mm
156 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features High Impact Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Profile Extrusion
PVC Cell Classification 16343
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Profiles
Users viewing this material also viewed the following: