Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS (Asia Pacific) PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | Molded; ASTM D882 |
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | |
Henkel Hysol EA 9330.3 Paste Adhesive System Non-slump, thixotropic adhesive with high peel strength and excellent environmental durability.Applications:Structural Repair Composite Bonding |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS - LINEAR LNP LUBRICOMP* OP005XXC is a compound based on PPS - Linear resin containing 25% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS (Asia Pacific) LNP* LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.68 GPa @Thickness 3.20 mm |
389 ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron XU 73120.00 Polycarbonate Resin Overview: XU 73120.00 Experimental Polycarbonate Resin is a high flow ignition resistant PC blend that contains no chlorinated or brominated additives. This resin is specifically designed to offer e.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific) |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region... |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
Tensile Modulus | 2.68 GPa @Temperature -40.0 °C |
389 ksi @Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | ASTM D-638 |
Axiall ProTherm® 4351 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4351 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial grade pipe requiring high heat deflection temperatures and excellent chemical resi.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |