Polymer Property : Tensile Modulus = 40.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 40.0 GPa
5800 ksi
ASTM D-638
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Tensile Modulus 40.0 GPa
5800 ksi
ASTM D-638
PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Tensile Modulus 40.0 GPa
5800 ksi
ASTM D 638
RTP Company RTP 1089 Polybutylene Terephthalate (PBT), Carbon Fiber
Tensile Modulus 40.0 GPa
5800 ksi
ASTM D638
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide..