Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy Molding Compound , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexMC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide range of applications.Information provided by Hexcel
Mechanical Properties Metric English Comments
Tensile Strength at Break 300 MPa
43500 psi
ASTM D638
Tensile Modulus 40.0 GPa
5800 ksi
ASTM D638
Flexural Strength 400 MPa
58000 psi
ASTM D790
Flexural Modulus 30.0 GPa
4350 ksi
ASTM D790
Compressive Strength 350 MPa
50800 psi
ASTM D695
Compressive Modulus 35.0 GPa
5080 ksi
ASTM D695
Shear Strength 45.0 MPa
6530 psi
In-Line; ASTM D5379