Mechanical Properties Metric English Comments
Tensile Modulus 0.276 GPa
40.0 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-UR-110-W Polyurethane, Unspecified (PUR, Unspecified)
Information provided by PolyOne
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works.
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works..
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works.
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
Tensile Modulus 0.276 GPa
40.0 ksi
ASTM D638
ScanTube MFA Tubing
Information provided by ScanTube, Inc.
Tensile Modulus 0.276 GPa
40.0 ksi
ASTM D638
ScanTube PFA Tubing
Information provided by ScanTube, Inc.
Tensile Modulus 0.276 - 0.552 GPa
40.0 - 80.0 ksi
Master Bond LED401 One Component LED Curable Adhesive System
Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In..
Tensile Modulus 0.276 - 0.552 GPa
40.0 - 80.0 ksi
Master Bond LED403Med USP Class VI, One Component, LED Curable System
Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi..
Tensile Modulus 0.276 GPa
40.0 ksi
1 mm/min
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay..
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
ITW Plexus Plexus™ MA925 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works.
Tensile Modulus 0.276 - 0.448 GPa
40.0 - 65.0 ksi
ASTM D638
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Tensile Modulus 0.276 GPa
40.0 ksi
TM R050-36
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin
Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro..