Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Mixed
Viscosity 40000 - 60000 cP
40000 - 60000 cP
B
130000 - 160000 cP
130000 - 160000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.1 - 13.8 MPa
1750 - 2000 psi
Elongation at Break 35 - 45 %
35 - 45 %
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
Shear Strength 8.96 - 12.4 MPa
1300 - 1800 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 40 - 45 min
40 - 45 min
Descriptive Properties Value Comments
Color White
Fixture Time 70-75 minutes
Gap Filling Max 0.375 in
Mix Ratio 10:1