Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.78 GPa | 403 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ E-PC CB Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments. Nemcon E-PC CB is a carbon black-filled polycarbonate characterized by consistent moldability, recyclability,.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 507XT PA6, DRY Description: Unreinforced polyamide 6, heat stabilized, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rod.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ASTM D-638 |
Axiall 3152 Rigid PVC, Extrusion Georgia Gulf 3152 is a twin screw powder blend NSF approved for the extrusion of potable water and drain waste and vent pipe application.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Tensile Modulus | 2.78 GPa | 403 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |