Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 56.0 GPa @Temperature 23.0 °C |
8120 ksi @Temperature 73.4 °F |
0°, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon Fiber Designation: C280T4; Twill 4x4Information provided by HexCel |
|||
Tensile Modulus | 56.0 GPa | 8120 ksi | RT; Dry; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |