Tensile Modulus 56.0 GPa

@Temperature 23.0 °C
8120 ksi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon
Fiber Designation: C280T4; Twill 4x4Information provided by HexCel
Tensile Modulus 56.0 GPa
8120 ksi
RT; Dry; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel