Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Eurotec
Trade Name Tecolen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Processing Properties Metric English Comments
Processing Temperature 200 - 240 °C
392 - 464 °F
Feed Temperature <= 60.0 °C
<= 140 °F
Throat
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Hold Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Medium - Fast