Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | |
Radici Radilon® S USX200 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D4894 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D4894 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Modulus | 0.600 - 0.700 GPa | 87.0 - 102 ksi | DIN 53457 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 246M PA66, Conditioned Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.600 - 0.800 GPa @Temperature 100 °C |
87.0 - 116 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BFZ 3 PA6 Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Tensile Modulus | 0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
DSM Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4180 black 9992 PA1010 Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4180 nat PA1010 Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resist.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4181 black PA1010 Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | DIN 53 457 |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | TD |
BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air Information provided by BASF |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | Sintered Molding; ASTM D638 |
3M Dyneon™ TF 1641 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | Sintered Molding; ASTM D638 |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | Sintered Molding; ASTM D638 |
3M Dyneon™ TF 1620 PTFE Meets ASTM D4894 Type IV, Grade 2 resinSemi-free-flowing compression molding powderHigh bulk densityGood for large billets and thin walled isostatic moldingsVery dense polymer structure, similar to .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
Unitika EX-1030 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |