Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.31 GPa | 1350 ksi | ASTM D638 |
PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Tensile Modulus | 9.31 GPa | 1350 ksi | ASTM D638 |
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products |
|||
Tensile Modulus | 9.31 GPa | 1350 ksi | ASTM D638 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Tensile Modulus | 9.31 GPa | 1350 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 9.31 GPa | 1350 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry) Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f.. |